赵立华,段渝平.高强度合金结构钢与高强度铝合金防护层的耐霉性研究[J].装备环境工程,2015,12(4):82-88. ZHAO Li-hua,DUAN Yu-ping.Mould Resistance of Protective Layer on High-strength Alloy Structural Steel and High-strength Aluminum Alloy[J].Equipment Environmental Engineering,2015,12(4):82-88.
高强度合金结构钢与高强度铝合金防护层的耐霉性研究
Mould Resistance of Protective Layer on High-strength Alloy Structural Steel and High-strength Aluminum Alloy
投稿时间:2015-06-01  修订日期:2015-08-15
DOI:10.7643/issn.1672-9242.2015.04.016
中文关键词:  高强度合金结构钢  高强度铝合金  防护层  霉菌试验
英文关键词:high-strength alloy structural steel  high-strength aluminum alloy  protective coating  mould test
基金项目:
作者单位
赵立华 1. 西南技术工程研究所,重庆 400039;2. 国防科技工业自然环境试验研究中心,重庆 400039 
段渝平 1. 西南技术工程研究所,重庆 400039;2. 国防科技工业自然环境试验研究中心,重庆 400039 
AuthorInstitution
ZHAO Li-hua 1. South West Institute of Technical Engineering, Chongqing 400039, China;2. The Natural Environmental Test and Research Center of Science, Technology and Industry for National Defense,Chongqing 400039, China 
DUAN Yu-ping 1. South West Institute of Technical Engineering, Chongqing 400039, China;2. The Natural Environmental Test and Research Center of Science, Technology and Industry for National Defense,Chongqing 400039, China 
摘要点击次数:
全文下载次数:
中文摘要:
      目的 研究高强合金结构钢和高强铝合金防护层的耐霉菌腐蚀能力。方法 以高强合金结构钢和高强铝合金两种材料为基材分别制备不同防护层, 按GJB 150.10A—2009进行实验室霉菌试验, 评定防护层的长霉等级。结果 两种材料的不同防护层中, 除润滑油涂层和阳级氧化层的长霉等级为0~1级外, 炮油涂层、 涂漆层、 镀锌层或锌镍合金层长霉等级均在2~3级。结论 高强合金结构钢润滑油涂层耐霉性能良好, 镀锌层或锌镍合金层、 涂漆层、 炮油涂层耐霉性能较差; 高强铝合金阳级氧化层耐霉性能良好, 炮油涂层、 涂漆层耐霉性能较差。
英文摘要:
      Objective To study the mould resistance of protective layers on high-strength alloy structural steel and high-strength aluminum alloy. Methods Different protective layers were prepared on high-strength alloy structural steel and high-strength aluminum alloy. Laboratory mould tests were carried out according to GJB 150.10A-2009 to evaluate the mould growth level on the protective layers. Results The mold levels of lubricant coating and anode oxidation layer on high-strength alloy structural steel and high-strength aluminum alloy were in the range of grade 0 ~ 1; the mold level of gun oil coating, paint coating, zinc layer or zinc nickel alloy layer moldy grade were in the range of grade 2~3. Conclusion For high-strength alloy structural steel substrate, lubricant coating had good mould resistance, while galvanized layer or zinc alloy layer, paint coating and gun oil coating had poor mould resistance. For high-strength aluminum alloy substrate, anode oxidation layer had good mould resistance, while gun oil coating and paint coating had poor mould resistance.
查看全文  查看/发表评论  下载PDF阅读器
关闭

关于我们 | 联系我们 | 投诉建议 | 隐私保护 | 用户协议

您是第11998540位访问者    渝ICP备15012534号-5

版权所有:《装备环境工程》编辑部 2014 All Rights Reserved

邮编:400039     电话:023-68792835    Email: zbhjgc@163.com

视频号 公众号